In Config C, one PXS128 drives each 490 × 1040 mm sheet. Total point count is unchanged; what changes is how much hardware you mount around the test area.
- —180 × 180 mm, under 200 g
- —One 4096-point sheet per unit
- —Half the collector count of Config B
- —20 Hz · 12 bit
Prices are quoted per configuration; no list prices are published.
Parts it is specified with
Film, collectors and software are quoted as one chain — the sheet count follows the surface size.
4096-point sensing film
Sensing principle: Piezoresistive · Thickness: 0.3 mm
Compact 4096-point collector
Model: PXS064mini · Dimensions: 90 × 40 mm
One session, all sheets
Platform: Windows desktop application · Input: Multiple collectors via docking hub
Configurations that include it
Real projects, without the names
Configuration, method and finding are published as delivered. Client identity stays with the customer — that is the only way these records get approved at all.
20,480 points across a 2.5 m² blade panel
Five long sheets and ten compact collectors merged into one continuous map over 1040 × 2480 mm, then compared against the aerodynamic model.
Bond-line pressure during spar cap bonding
Adhesive pressure mapped along the bond line before cure, replacing a trial-and-error shim routine.
Press platen uniformity before a curing change
40,960 points across ten sheets measured platen flatness under load, so the process change was decided on data rather than a sample.
Why it is specified this way
Selection notes and field measurements from our own test work.
Is 20 Hz enough for blade pressure measurement?
A 20 Hz sampling rate rules out vibration and transient work — and that is exactly why it is the
Choosing a flexible sensing film: range, array density and encapsulation
Three parameters constrain each other. Range headroom, array density and encapsulation are usual
The measurements this part is specified for
Bond-line pressure, read before cure
A press reporting the correct total force can still leave half a bond line starved. The number that matters…
Contact pressure across a bolted joint
Torque is an input, not a result. Two joints tightened to the same torque can carry very different pressure…
The rest of the range
4096-point sensing film
Sensing principle: Piezoresistive · Thickness: 0.3 mm
Compact 4096-point collector
Model: PXS064mini · Dimensions: 90 × 40 mm
One session, all sheets
Platform: Windows desktop application · Input: Multiple collectors via docking hub
Config A — 40,960 points
Sensing sheets: 10 × 490 × 520 mm · Collectors: 10 × PXS064mini
Config B — 20,480 points
Sensing sheets: 5 × 490 × 1040 mm (active 487 × 1034 mm) · Collectors: 10 × PXS064mini (two per long sheet)
Config C — 20,480 points
Sensing sheets: 5 × 490 × 1040 mm (active 487 × 1034 mm) · Collectors: 5 × PXS128 (one per long sheet)